Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 11.0 - 850 cm | 4.33 - 335 in | Average value: 150 cm Grade Count:8 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Spiral Flow | 11.0 cm @Thickness 1.00 mm |
4.33 in @Thickness 0.0394 in |
375°C nozzle, 180°C tool |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Spiral Flow | 11.0 cm @Thickness 1.00 mm |
4.33 in @Thickness 0.0394 in |
375°C nozzle, 180°C tool |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |