Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 47.0 - 468 cm | 18.5 - 184 in | Average value: 135 cm Grade Count:5 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Spiral Flow | 47.0 cm @Temperature 220 °C |
18.5 in @Temperature 428 °F |
ASTM D3123 |
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi.. |