Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 16.0 cm @Thickness 1.00 mm |
6.30 in @Thickness 0.0394 in |
380°C nozzle, 180°C tool |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |