Polymer Property : Spiral Flow = 6.50 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 16.5 cm

@Thickness 1.00 mm
6.50 in

@Thickness 0.0394 in
385°C nozzle, 180°C tool
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..