Physical Properties Metric English Comments
Spiral Flow 68.6 cm
27.0 in
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 68.6 cm
27.0 in
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne