Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 20.3 cm | 8.00 in | Equistar test |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |