Polymer Property : Spiral Flow = 8.94 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 22.7 cm

@Thickness 1.00 mm
8.94 in

@Thickness 0.0394 in
recommended processing conditions
Victrex® PEEK 150PF Easy Flow
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, ..