Polymer Property : Brookfield Viscosity = 150000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 150000 cP

@Temperature 0.000 °C
150000 cP

@Temperature 32.0 °F
ASTM D2983
Mitsui LUCANT™ HC-600 Synthetic Oil
LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity o..