Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 170000 cP @Temperature 32.0 °C |
170000 cP @Temperature 89.6 °F |
ASTM D2983 |
ExxonMobil SpectraSyn Ultra™ 1000 High VI Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high visco.. |