Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 450000 - 2.00e+6 cP

@Temperature 25.0 °C
450000 - 2.00e+6 cP

@Temperature 77.0 °F
322 Hardener; HBF, Helipath @ 5rpm, T-Bar Spindle E
Lord Adhesives 320 / 322 Epoxy Adhesive
LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides ..