Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 50 cP @Temperature 23.9 °C |
50 cP @Temperature 75.0 °F |
Part A |
BCC Products Proto-Kast BC 8163 Urethane Casting BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and.. |
|||
Brookfield Viscosity | 50 cP @Temperature 23.9 °C |
50 cP @Temperature 75.0 °F |
Part B; ASTM D2393 |
BCC Products BC 8990 Polyurethane Elastomer BC8990 is a two-component urethane elastomer compound specifically designed for general purpose molding and casting of various shapes. This product is a safe, easy-to-handle, room temperature mixing.. |