Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 400000 - 820000 cP

@Temperature 25.0 °C
400000 - 820000 cP

@Temperature 77.0 °F
310A Resin; HBF, Helipath @ 5rpm
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive
Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer..