Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | <= 1.30 g/cc | <= 1.30 g/cc | ASTM D792, A |
S&E Specialty Polymers XP23-45MG PVC Description: PVC weatherable, integral colored, filledApplication: Body side molding end caps and extruded skin compound which meets Chrysler MSDC 543 and Ford WSK-M4D689-A3Information provided by .. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Radici Radilon® A RV250 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | TM R050-16 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
2074A Polyurethane-based Biomedical Elastomer |
|||
Specific Gravity | 1.30 g/cc @Temperature 23.0 °C |
1.30 g/cc @Temperature 73.4 °F |
ISO 1183 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Specific Gravity | 1.30 - 1.36 g/cc | 1.30 - 1.36 g/cc | ASTM D 792 |
Karina E 18/35-FC-LMP Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Sylvin Technologies 8940-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Sylvin Technologies 9925-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | True |
Shin-Etsu Silicones X-52-854 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Teknor Apex APEX® 80851-F Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Forms: Pellets Uses Wire and Cable ApplicationsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Samyang Tribit® 1510 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1510 is a middle viscosity grade.Informatio.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 94-A0098A-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® 350U PBT (Asia Pacific) Impact modified, UV stabilised, flame retardant polyester with an internal glowwire rating of 850C on 1.6mm flat plaques.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ FTA-50-P Concentrate Based In LLDPE DescriptionPOLYBATCH® FTA-50-P is the next generation antiblock masterbatch to POLYBATCH® F-50-AP (50% DE in LLDPE). This masterbatch contains 50% film grade talc based in LLDPE. POLYBATCH® FTA.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Trelleborg S662 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
Axiall 10703 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 80°C at a 15 mil wall thickness.Information provided b.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | (Dry) |
Radici Radilon® A CF350 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, .. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |