Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP320E Cotton Fabric Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500†|
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D 792 |
Karina BR-11 White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 34 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 207 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions. Improved .. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF .. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 41 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 42 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity. Lower mechanical and electrical properties than PF CP 41.Information.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AU-050595 PVC Compound Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 31 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity.Information provided by Hippe. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall EX1264 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 10840 Wire & Cable Flexible PVC High gloss jacket and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 11800 Wire & Cable Flexible PVC Designed for 75°C rated cords and cord sets and other general purpose insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 15880-02 Wire & Cable Flexible PVC TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 38601 Coax & Telecom Flexible PVC CATV and general purpose jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8800 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 2161A Wire & Cable Flexible PVC Flame retardant, oil resistant, 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.00 - 1.40 g/cc | 1.00 - 1.40 g/cc | ASTM D792 |
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 46234B Flexible PVC Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.40 g/cc | 1.34 - 1.40 g/cc | ASTM D 792 |
Karina 900D10/120-IS-PO White PVC Compound PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |