Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.0400 - 0.0450 g/cc | 0.0400 - 0.0450 g/cc | |
P & P Technology Expanded Polyurethane Closed Cell Sponge Specification Description: Metweave is a lamination of PPT conductive fabric and closed cell polyurethane. Cells: Closed cell, cell surface finish.Performance: Oil, Weather & Ozone ResistantInformation provided b.. |