Physical Properties Metric English Comments
Specific Gravity 0.0550 - 0.0650 g/cc
0.0550 - 0.0650 g/cc
P & P Technology Polyester Polyurethane Foam
Description- High performance acoustic and dust filtration foam with a density of 60 Kg/cubic meter with excellent fire resistance properties. Used in heating, ventilation, electronic, aeronautic, a..