Physical Properties Metric English Comments
Specific Gravity 0.550 g/cc
0.550 g/cc
Part B; TM R050-16
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti..