Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.680 - 0.880 g/cc | 0.680 - 0.880 g/cc | |
Parker Chomerics CHO-BOND 1086 Conductive Caulk/Sealant Chomerics two-component conductive epoxy caulks provide excellent adhesion to dissimilar substrates and can be used in lap or butt joint applications. They feature large silver-plated-copper particl.. |
|||
Specific Gravity | 0.680 g/cc | 0.680 g/cc | |
Permabond CleanerA Surface Cleaner Permabond Cleaner A is a general purpose industrial cleaner for cleaning and degreasing surfaces prior to bonding with any Permabond adhesive. Where surfaces are greasy or dirty, wiping with CLEANER.. |
|||
Specific Gravity | 0.680 - 0.880 g/cc | 0.680 - 0.880 g/cc | |