Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.710 - 0.750 g/cc | 0.710 - 0.750 g/cc | |
Cos46 Cork/Synthetic Rubber Sheet Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot.. |
|||
Specific Gravity | 0.710 g/cc | 0.710 g/cc | |
Chesterton 294 CSD Industrial Degreaser Description: Chesterton® 294 CSD is a fast acting, industrial degreaser for critical equipment. It contains no chlorinate, aromatic or solvents of questionable toxicity. Designed to quickly penetra.. |