Specific Gravity 0.800 - 0.820 g/cc
0.800 - 0.820 g/cc
Michelman® Wax Dispersion 40 Solvent dispersion
Description: Solvent dispersion of paraffin waxUsage: Wax Dispersion 40 is most effective as a water repellent aid and also has some slip and release properties in solvent applications. Wax Dispersi..