Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.822 g/cc | 0.822 g/cc | ASTM D792 |
Polymax® Maxelast® C4800 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |
|||
Specific Gravity | 0.822 g/cc | 0.822 g/cc | ASTM D792 |
Polymax® Maxelast® C4803 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |
|||
Specific Gravity | 0.822 g/cc | 0.822 g/cc | ASTM D792 |
Polymax® Maxelast® C4805 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |
|||
Specific Gravity | 0.822 g/cc | 0.822 g/cc | ASTM D792 |
Polymax® Maxelast® C4807 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |