Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.833 g/cc | 0.833 g/cc | d<sup>20</sup><sub>4</sub>; Anton Paar density meter |
Mitsui LUCANT™ HC-40 Synthetic Oil LUCANT®, a hydrocarbon-based synthetic oil having no polar groups, is a co-oligomer of ethylene and -olefin. It possesses surpassing resistance to heat and cold and lower dependence of viscosity.. |
|||
Specific Gravity | 0.833 g/cc | 0.833 g/cc | 50°C |
ChevronTexaco 22 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |
|||
Specific Gravity | 0.833 g/cc | 0.833 g/cc | ASTM D-4052 |
ConocoPhillips Hydroclear® 6 Ultra-Clean Spindle Oil Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o.. |