Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.835 g/cc | 0.835 g/cc | ASTM D-792 |
Saint-Gobain Norton® PMP Film Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail.. |