Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Network Polymers Softflex® 0250
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Specific Gravity 0.890 g/cc
0.890 g/cc
Radici Heraflex® P 40D 11 I HF 1530 Modified Polypropylene
Shore hardness: 40D (3s)Shiny surface, very flexible even at very low T°C (to -30°C), good resistance to weather conditions, very light and recyclableApplication examples: hiding soft, winter foot..
Specific Gravity 0.890 g/cc
0.890 g/cc
Shin-Etsu Silicones KF-7002 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP 1225 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1702C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1766-R1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1838-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1878B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-2112 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP 1213A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP 1227A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1349A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-2870M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.890 - 0.910 g/cc
0.890 - 0.910 g/cc
ASTM D792
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Specific Gravity 0.890 g/cc
0.890 g/cc
ExxonMobil Mobil Clean 20W-50 Motor Oil
Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D1505
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting..
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 1183/1
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D 792
RTP Company RTP 2700 S-30A MD NATURAL Saturated Styrenic Block Copolymer ISO 10993 Tested
ISO 10993 is used to evaluate the biocompatibility of medical devices. Consult RTP Company for more details.
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Specific Gravity 0.890 g/cc
0.890 g/cc
Part B
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Teknor Apex Monprene® MP-2604B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
PolyOne Synprene® IT 38-034 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclaimer: A..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla..
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 1183/1
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by..
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D 792
RTP Company RTP 2700 S-40A Saturated Styrenic Block Copolymer, General Purpose