Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.897 g/cc | 0.897 g/cc | Woven Density |
Saint-Gobain Chemlam® RL® RL6000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sintered PTFE for.. |