Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.963 g/cc | 0.963 g/cc | ASTM D1505 |
Chevron Phillips Marlex® EHM 6004 High Density Polyethylene, Blow Molding This high molecular weight, ethylene homopolymer is tailored for lightweight blow molded containers that:Require excellent stiffnessRequire exceptional processabilityAre durable and recyclable for s.. |
|||
Specific Gravity | 0.963 g/cc | 0.963 g/cc | at 60°F |
Duratherm G Polyalkylenev Glycol Heat Transfer Fluid Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improv.. |