Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.019 g/cc | 1.019 g/cc | |
Northstar Polymers PPA-059 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.019 g/cc | 1.019 g/cc | |
Dow VORANOL™ 4701C Polyether Polyol VORANOL™ 4701C polyether polyol is a high reactivity capped triol. Its nominal 4800 molecular weight and primary hydroxyl content make it well suited for the production of high resiliency, flexibl.. |