Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.021 g/cc | 1.021 g/cc | |
Dow VORANOL™ CP 4711 Polyol VORANOL™ CP 4711 polyol is a medium reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formu.. |