Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.031 g/cc | 1.031 g/cc | |
Northstar Polymers PPF-028 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.031 g/cc | 1.031 g/cc | |
Dow SPECTRIM™ 35B-S Polyol SPECTRIM™ 35B-S reaction moldable polymer is one component (SPECTRIM™ 35A is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology dev.. |
|||
Specific Gravity | 1.031 g/cc | 1.031 g/cc | |
Dow SPECTRIM™ 50B-S Polyol SPECTRIM™ 50B-S reaction moldable polymer is one component (SPECTRIM™ 35B-S is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology d.. |