Polymer Property : Specific Gravity = 1.056 g/cc
Polymer Property :
Specific Gravity =
1.056 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
1.056
g/cc
1.056
g/cc
Northstar Polymers MPA-135 MDI Ether Prepolymer
Information provided by Northstar Polymers.