Polymer Property : Specific Gravity = 1.065 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.065 g/cc
1.065 g/cc
Northstar Polymers PND-011 Polyether Curing Agent
Information provided by Northstar Polymers.
Specific Gravity 1.065 g/cc
1.065 g/cc
15/15°C
ChevronTexaco Texcool® EXL 304
In service Texcool EXL products provide:A 32,000 hour/8 years of service life with no inhibitor additions neededNo regular inhibitor testing requiredExcellent heat transfer and corrosion protection ..
Specific Gravity 1.065 g/cc
1.065 g/cc
Dow VORANOL™ CP 450 Polyol
VORANOL™ CP 450 polyol is a glycerine propoxylated polyether triol.Information provided by Dow