Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.117 g/cc | 1.117 g/cc | ASTM D792 |
Ovation Polymers OPTRENE 30GF Polypropylene, 30% Glass Reinforced Properties of chemically coupled glass reinforced (30%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All .. |