Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.165 g/cc | 1.165 g/cc | ISO 1183 |
Nanocyl PLASTICYL™ PA1501 Polyamide 66 - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |