Physical Properties Metric English Comments
Specific Gravity 1.246 g/cc
1.246 g/cc
ASTM D792
PolyOne Lubri-Tech™ NL-20GF/05T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedInformation provided by PolyOne Corporation.
Specific Gravity 1.246 g/cc
1.246 g/cc
Hexcel® HexPly® M65 Bismaleimide Resin
HexPly® M65 is a bismaleimide resin that cures via an addition reaction in a toughened two-phase thermoset matrix with no condensation by-products. HexPly® M65 is a controlled flow polyimide resin..