Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.256 g/cc | 1.256 g/cc | Woven Density |
Saint-Gobain COHRlastic® 1015 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |