Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.291 g/cc | 1.291 g/cc | ASTM D792 |
PolyOne Edgetek® BB-20GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |