Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.315 g/cc | 1.315 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ NL-15CF-15GF/5M Nylon 6/12, Carbon/Glass Filled
(discontinued **) Description/Features:Carbon Fiber ReinforcedGlass Fiber ReinforcedMolybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.315 g/cc | 1.315 g/cc | ISO 1183 |
Lanxess Durethan® BKV 20 FN20 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 20% glass fibers, injection molding, halogen-free flame retardantInformation provided by LANXESS. |