Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.335 g/cc | 1.335 g/cc | Woven Density |
Saint-Gobain COHRlastic® 1115 Abrasion Resistant Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Specific Gravity | 1.335 g/cc | 1.335 g/cc | |
Hexcel® HexPly® F155 Epoxy Resin HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly.. |