Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.325 - 1.335 g/cc | 1.325 - 1.335 g/cc | |
Dow UVI-6992 Photoinitiator UVI-6992 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6992 photoinitiator is used to UV-cure CYRACURE™ cycloaliphati.. |