Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.423 g/cc | 1.423 g/cc | ASTM D792 |
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |