Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
PolyOne Edgetek® PK-40CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8318-1 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Shinil Chemical SHINCON PPS-CF, Comp. "Y"-2 LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON 9X08403C Liquid Crystal Polymer (LCP) LNP* STAT-KON* 9X08403C is a compound based on Liquid Crystal Polymer (LCP) resin containing Carbon Fiber. Added features of this material are: Clean Compounding System, High Temperature, Flame Re.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Silberline Sparkle Silver® 5242-AR Sparkle Silver® 5242-AR is a medium, bright, non-leafing aluminum pigment with a narrow particle size distribution. It provides exceptional brightness and is acid resistant.Applications: Automoti.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | |
Sylvin Technologies 5042N PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SSH 5509 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3 Agency Ratings: BS 6746; IEC 60502; JIS 6723 Forms: .. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
E-Polymers SEPAZ® LB40 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Specific Gravity | 1.46 g/cc | 1.46 g/cc | Part B; TM R050-16 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |