Polymer Property : Specific Gravity = 1.546 g/cc
Polymer Property :
Specific Gravity =
1.546 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
1.546
g/cc
1.546
g/cc
ASTM D792
PolyOne Therma-Tech™ NJC-8500 Nylon 12 (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.