Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | Method A; ASTM D792 |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Specific Gravity | 1.64 - 1.70 g/cc | 1.64 - 1.70 g/cc | ASTM D 792 |
Karina 18/219-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Daelim H&L Plavis-G40 CM 40% Graphite Filled Aromatic Polyimide Bearing Compression Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbo.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |