Physical Properties Metric English Comments
Specific Gravity 1.896 g/cc
1.896 g/cc
Woven Density
Saint-Gobain Chemlam® 3300 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite
Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluorop..