Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.942 g/cc | 1.942 g/cc | Woven Density |
Saint-Gobain Chemlam® 3320 High Mechanical Performance Industrial Laminate Description: Chemlam® Silver Ultra is the best mechanically performing series of Chemfab® industrial laminates. Chemlam® Silver Ultra composites feature uniform thickness, multi-layer cast .. |