Polymer Property : Specific Gravity = 10.8 g/cc
Polymer Property :
Specific Gravity =
10.8 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
10.8
g/cc
10.8
g/cc
Calculated
Plansee MoRe5 Molybdenum-Rhenium
Highly ductile alloy, even below room temperature.Applications: thermocouple wiresInformation provided by Plansee.