Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 18.9 g/cc | 18.9 g/cc | Calculated |
Plansee WLZ Lanthanum Oxide and Zirconium Oxide-doped Tungsten A non-radioactive Tungsten alloy suitable for the manufacture of cathodes used in high-load environments.Characteristics:High creep resistanceGood stability at extremely high temperaturesGood igniti.. |