Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 19.2 g/cc | 19.2 g/cc | Calculated |
Plansee WL10 Lanthanum Oxide-doped Tungsten Tungsten alloy suitable for use as ion sources, lamp electrodes and welding electrodes.Characteristics (compared to pure tungsten):Improved creep resistanceHigher recrystallization temperatureMachin.. |
|||
Specific Gravity | 19.2 g/cc | 19.2 g/cc | Calculated |
Plansee WL-S Lanthanum Oxide-doped Tungsten Tungsten alloy suitable for use as support rods in high-pressure discharge lamps.Characteristics (compared to other tungsten-lanthanum oxide alloys):More fine-grained microstructureHigher strength a.. |