Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.125 - 2.875 g/cc | 2.125 - 2.875 g/cc | |
Parker Chomerics Tecknit Teckfip™ FIP-C Formed in Place Conductive Elastomer Description: This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommunications base stati.. |