Physical Properties Metric English Comments
Specific Gravity 2.24 - 2.27 g/cc
2.24 - 2.27 g/cc
ASTM D792
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic
Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon.